1.Product features:
This product is a kind of light green powder solid and is prepared with nickel salt, cobalt salt, accelerant, stabilizer, penetrant, dust inhibitor, disperser and surface activator. Compared with conventional sealant, it has the following advantages:
1) The tank liquid has strong buffering capacity and good impurity ion interference resistance.
2) Tank liquid group features easy control, wide parameter range and less influence to sealing effect caused by process flotation and technical parameter change of previous process.
3) It has fine composition and selected suitable surface activator avoids common ash hanging and other disadvantages.
4) After sealing, the surface luster and hardness of profile have been improved.
2.Tank composition:
HA—01 2.5~3.5 g/L
Deionized water Margin
3.Technical parameters:
Ni2+ content 0.8~1.3 g/L
F- content 0.3~0.7 g/L
Temperature 20~35℃
PH value 5.5~6.6
Time 1um/min
4.Packing and storage:
The products are packed with 20kg cartons, lined with single layer or double layer plastic bags. During storage and transportation, it shall be resistant to moisture.
A freshly anodized aluminum part can have the right color and appearance while its sealing quality still needs checking. We develop Aluminum surface treatment additives with that final production step in mind. Our Normal temperature sealant product category covers chemical treatments considered for sealing compatible anodic coatings near room temperature. We select the grade around your coating, coloring process, equipment, and required performance, then confirm the complete treatment and inspection plan.
On this page, sealant means a chemical treatment used to seal the pores of an anodized aluminum surface. It is part of the finishing line. We assess it alongside the anodizing conditions, any coloring stage, rinsing, and the requirements for the finished component.
Sulfuric acid anodizing produces a coating with a porous outer structure. Those pores are useful during suitable coloring processes, but the finished product may require sealing to improve its resistance to unwanted absorption and environmental exposure. We confirm that requirement for the actual application.
You may see the terms normal temperature sealant, Room temperature anodizing sealant, or cold sealing agent used in product discussions. The selected grade's instructions must define what the temperature description means. A workshop that feels comfortable to an operator does not necessarily provide the required bath condition.
We also establish the full treatment sequence. A lower-temperature first stage may require a defined rinse, later conditioning, or another treatment before the product is ready for inspection and release. We do not reduce a multistage process to the temperature of one tank.
The chemistry needs its own confirmation. Cold-sealing products can use different formulations, and the temperature label does not identify nickel content, fluoride content, cobalt content, or restricted-substance status. Those questions belong in the documentation for the chosen grade.
Before selection, we ask for the alloy, anodizing route, coating thickness, color, existing sealing method, and customer specification. We also need to know when the parts will be tested and what happens between sealing and packing. That information helps us build an evaluation that reflects production.
Our aim is a sealing stage that can be controlled and verified. An attractive sample matters, but we approve the process against agreed coating and appearance requirements rather than judge it from appearance alone.
A simple way to picture an anodic coating is as a surface containing many very small channels. Sealing changes the condition of those channels so they provide less access for unwanted material. The exact reactions depend on the sealing system.
In hydrothermal sealing, hot water reacts with the anodic oxide and produces hydrated material that helps close the pores. Cold-sealing systems use chemistry that can develop a sealing effect at a lower temperature. They should not be treated as identical processes with only a different heater setting.
As an industry example, research on nickel-fluoride-based cold sealing has identified reaction products containing aluminum, nickel, and fluoride within the treated coating. This explains why the active chemical balance matters. It does not establish that our selected grade contains those ingredients or follows the same reaction path.
We assess both the coating and the bath. Coating thickness, pore condition, prior treatment, coloring, and the time between stages can influence the evaluation. A suitable sealant cannot be expected to correct every defect already present in the anodic film.
Contact with the working solution must also be consistent. Part orientation, trapped air, rack spacing, and solution movement can affect access. A successful test on an easy flat coupon does not establish the result in a recessed component or along a large production load.
We define the rinse and any required conditioning after the sealing bath. Some cold-sealing processes continue to change after the initial immersion. The agreed test timing therefore forms part of the process definition, rather than being left to whichever shift happens to perform the check.
We also distinguish pore sealing from color performance. Suitable sealing can contribute to the completed dyed finish, but the dye, anodic coating, exposure conditions, and other treatments still matter. We evaluate color compatibility and the required durability separately where the application demands it.
Technical background: Li Yi and colleagues, Mechanism of Cold Sealing of Anodic Oxide Films on Aluminum, Journal of Chinese Society for Corrosion and Protection, 1992; Hyunbin Jo and colleagues, Low Temperature Sealing of Anodized Aluminum Alloy for Enhancing Corrosion Resistance, Materials, 2020. These describe investigated systems, not Huaao product test results.
When we consider a Normal temperature sealant for aluminum anodizing, we look beyond the temperature label. We want to know whether it can meet the agreed sealing requirements, preserve the intended appearance, and fit the available production sequence.
Lower bath temperature can reduce the theoretical heating requirement compared with a hotter stage under otherwise similar conditions. Actual energy use depends on tank size, insulation, operating hours, loading, and the rest of the treatment. We compare the complete process before discussing a saving.
A lower-temperature bath still needs temperature control. Seasonal changes, incoming loads, circulation, and other heat sources can affect the liquid. Depending on the installation and grade, maintaining the working window may involve heating, cooling, or both.
These external examples show why we confirm the operating window for a named grade. They are not interchangeable formulations, equal-performance claims, or instructions for using our product.
| Published Reference Product | Published Sealing Category | Published Product Concentration | Published Temperature | Published Time Information |
|---|---|---|---|---|
| BONDERITE M-ED CS2 | Low-temperature metal-salt sealing | 4–6 g/L | 20–25°C | Not stated in the cited brochure |
| BONDERITE M-ED 30 | Metal-salt sealing | 4–6 g/L | 25–30°C | Not stated in the cited brochure |
| SurTec 343 Hardwall | Mid-temperature sealing | Not stated on the cited overview page | Can operate down to 88°C under the stated condition | 3 minutes per micrometre of coating thickness at that condition |
Sources: Henkel Japan, Anodizing Agents product brochure, July 2024, page 2; SurTec, Value-added Anodizing Portfolio, hot and mid-temperature sealing section. Henkel identifies its brochure figures as reference values. Confirm current grade-specific instructions and the full sequence before use.
We use such information to define the right questions for a trial. Required temperature, treatment time, coating thickness, chemical control, appearance, and later conditioning must be assessed together. A lower number in one column cannot establish the right process for your parts.
We focus on a workable bath-control method, repeatable treatment, compatibility with the coloring process, and a surface that meets the agreed inspection. We also assess rinsing and any risk of visible deposits because a process must satisfy both technical and appearance requirements.
Where reduced consumption, longer bath service, or fewer rejected parts is a project target, we agree a measurement plan. Those benefits must be established for the actual grade and production conditions. We do not attach a fixed saving or service-life claim to an unevaluated line.
We begin by reviewing the anodizing and coloring stages. Coating thickness and condition should be known, and the surface should reach sealing through the agreed rinse sequence. Problems carried from an earlier stage can affect both bath stability and the finished part.
We pay attention to drainage and transfer. Liquid carried on racks and parts can introduce material from the previous tank. Trapped liquid and inconsistent handling can also make one area of a component experience different conditions from another.
We confirm whether the selected sealing agent is supplied as a liquid, powder, concentrate, or part of a multicomponent system. Product concentration must be expressed on the correct basis. The quantity of supplied product is not automatically the concentration of every active ingredient in the working bath.
Where the chemistry requires individual active components to be measured, we follow that grade's analytical method. A general concentration reading cannot replace a required balance between components. Similarly, a clear bath does not prove that all chemical values are acceptable.
We record the actual bath temperature at a representative location. A room thermometer or heater setting is not enough. The operating record should also identify the load and relevant conditions so that a result can be connected to the treatment the parts received.
Bath pH describes one aspect of the chemical condition. We use the selected grade's instructions for measurement and adjustment, alongside any required active-component analysis. We do not copy a pH target or correction method from a different sealant.
Sealing time must be connected to the approved process and coating. Where the instructions relate treatment to film thickness, that thickness needs a suitable measurement. We also define when timing starts, how transfer is handled, and what follows immersion.
We review make-up water, rinse water, and contamination carried between stages. A conductivity reading can help monitor a change, but it does not identify every dissolved substance. The water specification and checking method must suit the selected sealing chemistry.
Tanks, pumps, filters, heaters, sensors, and seals need material compatibility with the formulation. We assess them using the product's technical and safety information. An installation that worked with one sealing product should be reviewed before introducing another.
We keep a practical record of analysis, additions, temperature, loads, treatment time, and test results. That record helps us investigate a change before making repeated chemical additions or extending the cycle without understanding the cause.
We agree the inspection method before product approval. The test must suit the coating, color, sealing process, and customer requirement. A method that works well for one finish may be unsuitable or difficult to interpret for another.
We also define sample conditioning and test timing. For a process that includes later treatment or a specified waiting period, the sample must complete that sequence. We record its history rather than compare results from parts tested at different stages.
| Assessment | Published Reference | Main Information Provided | Important Selection Point |
|---|---|---|---|
| Dye-spot assessment | ISO 2143:2017 | Estimates loss of absorptive power after sealing through dye absorption following acid pretreatment. | Deep colors and certain coating conditions fall outside its scope. |
| Admittance assessment | ISO 2931:2017 | Assesses the sealed coating through its electrical response. | Results from different sealing methods are not necessarily comparable. |
| Acid-immersion mass-loss assessment | ISO 3210:2025 | Measures mass lost after a specified acid exposure. | It is destructive; method choice and coating exclusions must be checked. |
Sources: International Organization for Standardization, official scope descriptions for ISO 2143:2017, ISO 2931:2017, and ISO 3210:2025. This comparison summarizes their purposes. It does not replace the complete methods or establish a common acceptance limit.
For dark dyed parts, we check whether a visual dye-spot method is applicable before relying on its result. ISO 2143 identifies exclusions and limitations involving color, alloy, coating thickness, and certain supplementary treatments. A test should not be used simply because it is familiar.
Admittance is an electrical measurement, not a direct reading of corrosion life. ISO 2931 notes that results obtained from different sealing methods are not necessarily comparable. We keep the process, coating, measurement conditions, and agreed interpretation connected to the reported value.
ISO 3210:2025 provides acid-immersion mass-loss methods with different pretreatment arrangements and application scopes. We specify which method is required and check that it applies to the coating. A report stating only that a sample passed a mass-loss test leaves important information unresolved.
We obtain acceptance criteria from the applicable customer specification or quality agreement. Method names alone do not provide every requirement for every application. Where a separate quality-label scheme is involved, its applicable edition and additional requirements also need review.
We inspect color, gloss, streaking, deposits, and water marks under agreed viewing conditions. Those observations complement sealing tests. An attractive surface does not demonstrate pore sealing, while a satisfactory technical result does not excuse an unacceptable decorative appearance.
Our trial plan includes representative material, colors, coating conditions, and difficult geometries. We compare repeated production where appropriate, rather than approve a process from one selected sample. Any claim about outdoor durability or service performance needs evidence relevant to that separate requirement.
When a sealing result changes, we first confirm that the sample and test procedure match the approved plan. We review coating thickness, color, conditioning history, measurement settings, and the test record. We then compare bath analysis, temperature, exposure, and recent additions. This sequence helps separate a treatment problem from a change in how the sample was prepared or assessed.
If deposits or streaks appear, we also inspect rinsing, drainage, drying, and the condition of incoming work. We avoid adjusting the bath from appearance alone. The corrected process should meet both the visible finish requirement and the relevant sealing assessment before it is accepted. Recording what changed makes the correction useful for later production rather than a one-time trial adjustment.
For windows, doors, curtain walls, and interior systems, we consider the final anodized finish and the customer's requirements. Profiles may be clear, dyed, or electrolytically colored. We evaluate the actual finish because the sealing method and test selection must fit that condition.
Long profiles also require practical attention to drainage, handling, and uniform exposure. We assess the completed process on representative sections and visible surfaces, including matching requirements where several pieces will be installed together.
Handles, trims, frames, and fittings often combine flat faces, curves, and recesses. We review whether the treatment reaches those areas and whether drying leaves an acceptable appearance. The trial should represent the part's shape and final color rather than an easy substitute.
For anodized covers, panels, and housings, we assess sealing alongside the intended appearance and later operations. Retained liquid, protected areas, and assemblies containing different materials deserve review. We do not assume that a grade accepted for an open profile suits every assembled component.
We consider anodized components where the sealing route fits the specified function. Customer requirements may involve cleaning resistance, appearance, wear, or another property. Those requirements need their own evaluation; a general pore-sealing result does not establish approval for every industrial use.
We also confirm whether sealing is appropriate for the particular coating and purpose. Functional anodized surfaces can have requirements that differ from decorative finishes. We begin with the part specification rather than apply the same sealing instruction to every anodized item.
At Jianli Huaao Technology Co., Ltd., we develop, produce, and supply chemical additives for aluminum profile surface treatment. We have worked in this field for more than two decades, combining product research with technical consulting. Our base is in the Huazhong Ecological Aluminum Demonstration Industrial Park in Jianli, Hubei.
Our production facilities, testing instruments, and quality assurance system support this work. We also serve as a standing council member of the China Non-Ferrous Metals Processing Industry Association. We connect this industry experience with the documentation and application evaluation required for the chosen grade.
Our product range includes low-, medium-, and high-temperature sealing agents, together with degreasing, etching, polishing, coloring, and passivation products. This broader process knowledge helps us discuss the sealing stage in relation to the surface it receives and the finished part it must deliver.
We define the supplied product and its intended application before discussing routine orders. Product release requirements should identify the relevant properties and test methods. These belong alongside, but remain distinct from, instructions for controlling the customer's working bath.
Raw-material identification, formulation control, mixing, inspection, and packaging are connected manufacturing requirements. We discuss the checks relevant to the selected Normal temperature sealant grade. A useful quality agreement identifies what is measured rather than rely on a broad statement about consistency.
Delivery documents should identify the grade, quantity, batch information, and agreed inspection requirements. The technical instructions and safety data sheet must correspond to the supplied material. Any additional report or document requirement should be confirmed before order acceptance.
We confirm production timing according to formulation, order quantity, and required testing. An application that still needs evaluation follows a different plan from an established grade with an agreed specification. Confirmed timing is recorded in the order agreement.
Payment terms may include T/T or L/C, subject to agreement. We confirm the payment stages, documents, and other accepted conditions in the contract. We do not apply an assumed deposit percentage or payment period to every customer.
We select packaging according to product form, chemical compatibility, safety information, and transport requirements. Suitable sealed drums or intermediate bulk containers may be considered for liquids; moisture-resistant packaging may apply to powder grades. The actual package is confirmed for the supplied product.
Sea freight and road transport can be assessed for suitable orders. Air shipment depends on product classification, packaging, carrier requirements, and route. Storage temperature and shelf life follow the grade's documentation, rather than assumptions based on its processing name.
Yes. We use the selected grade's documented working window and measure the bath itself. Seasonal conditions and production loading can move it outside that window. The need for heating or cooling depends on the installation and formulation.
We confirm compatibility for the actual coating, dye or electrolytic color, and treatment sequence. Color appearance and sealing quality both need checking. A result accepted for one shade or coloring route should not be assumed to cover all others.
Only if the selected process defines that as completion. Required rinsing, later conditioning, or additional treatment must be included before testing and release. We record that sequence so the sample history matches the agreed inspection method.
No. The temperature description does not establish composition. We confirm relevant chemical and restricted-substance information for the selected grade using its documentation. Any specific substance claim must be supported for that product.
No. We check the method's scope against the alloy, coating, color, sealing route, and later treatment. Dye-spot, admittance, and acid-immersion mass-loss assessments provide different information. The agreed inspection plan defines the suitable method and acceptance criteria.
It may reduce part of the heating demand, but we assess the complete production route. Compare energy, chemical use, treatment and conditioning time, accepted output, and rework. A lower first-stage temperature alone does not establish the overall saving.
Share your anodizing route, coating thickness, colors, current sealing method, and quality requirements so we can discuss a suitable Normal temperature sealant grade and a practical trial plan.